Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 557 °C | 1030 °F | |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Transformation Temperature, Tg | 557 °C | 1030 °F | |
Schott D 263® T eco Thin Borosilicate Optical Glass D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm.. |
|||
Transformation Temperature, Tg | 554 °C | 1030 °F | |
Schott N-BAK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 557 °C | 1030 °F | |
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 553 °C | 1030 °F | |
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 557 °C | 1030 °F | |
Schott WG295 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |