Schott D 263® T eco Thin Borosilicate Optical Glass

Category Ceramic , Glass , Optical
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott D 263® T eco Thin Borosilicate Optical Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm to 1.1 mm. D 263® T eco borosilicate glass is available in standard stock size sheets or can be custom cut into round or square shapes. D 263® T eco thin glass is used as a substrate glass for coatings or replacement for plastic for applications in the automotive and electronics industries D 263® T eco is manufactured without adding arsenic and antimony as refining agents. It has been used in touch panel displays, optocaps for diode lasers, and other optical applications.Information provided by SCHOTT North America.
Physical Properties Metric English Comments
Density 2.51 g/cc
0.0907 lb/in³
Thickness 30.0 - 1100 microns
1.18 - 43.3 mil
wide range available
Thermal Properties Metric English Comments
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 557 °C
1030 °F
Optical Properties Metric English Comments
Refractive Index 1.523

@Wavelength 588 nm
1.523

@Wavelength 588 nm
n<sub>d</sub>
Transmission, Visible 91.7 %

@Thickness 1.1 mm
91.7 %

@Thickness 0.043 in
T<sub>vD65</sub>
Electrical Properties Metric English Comments
Dielectric Constant 6.7

@Frequency 1e+6 Hz
6.7

@Frequency 1e+6 Hz
Copyright © lookpolymers.com All Rights Reserved