Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific) Super high impact ABS. Good low temperature toughness. High gloss. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C | 53.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6,6 IM 6040 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -20.0 - 150 °C |
53.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
CTE, linear, Parallel to Flow | 95.4 µm/m-°C @Temperature -20.0 - 150 °C |
53.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |