Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 17.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
9.89 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Verton UV00A PPA LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region. |