Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 74.4 µm/m-°C @Temperature -30.0 - 100 °C |
41.3 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM E 831 |
MRC Polymers NAXELL™ PC429MHI Polycarbonate, Impact Modified • Medium MFR• Good property retention, heat and dimensional stability• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants ca.. |
|||
CTE, linear, Parallel to Flow | 74.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare. |