Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 33.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6 LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite. |
|||
CTE, linear, Parallel to Flow | 33.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |