Polymer Property : CTE, linear, Parallel to Flow = 33.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 203 °F
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP COLORCOMP DX98550H PC
LNP* COLORCOMP* DX98550H is an unfilled Polycarbonate resin. Added features of this grade are: Low Extractable, Healthcare.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
18.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature 20.0 °C
18.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
18.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East)
LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
18.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature 20.0 °C
18.3 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m..
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
18.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding
Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 33.0 µm/m-°C
18.3 µin/in-°F
ISO 11359
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
CTE, linear, Parallel to Flow 33.0 µm/m-°C
18.3 µin/in-°F
ISO 11359
BASF Ultramid® A3EG3 BK00564 15% Glass Filled PA66 (Dry)
Ultramid A3EG3 BK00564 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
CTE, linear, Parallel to Flow 33.0 µm/m-°C
18.3 µin/in-°F
ISO 11359
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..
CTE, linear, Parallel to Flow 33.0 µm/m-°C
18.3 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
18.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 33.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
18.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON RX00327 PA 66
LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural.