Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 29.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.5 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF0059 PA 66 LNP THERMOCOMP* RF0059 is a compound based on Nylon 66 resin containing 25% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 29.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.5 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |