Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 42.3 µm/m-°C @Temperature 20.0 °C |
23.5 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Questra® QA805 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
CTE, linear, Parallel to Flow | 42.3 µm/m-°C @Temperature -30.0 - 30.0 °C |
23.5 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized. |