Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Questra® QA805 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Syndiotactic Polystyrene (SPS) , Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Questra® QA805 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are very different from conventional styrenics in structure, and properties, exhibiting excellent heat resistance with a melting temperature of 270.C, excellent moisture and chemical resistance together with a unique combination of exceptional electrical properties, toughness and processability. QUESTRA crystalline polymers are typically used as moldings, films, and fibers in Electronic, Electrical, Automotive, Consumer and Industrial, Filtration, Optical/photographic film and Specialty fiber/non-woven markets. QUESTRA QA805 is a 30% glass filled, impact modified, high temperature resistance polymer suitable for Consumer and Industrial applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM Data
Water Absorption 0.010 %
0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 105 MPa
15200 psi
ASTM Data
Tensile Strength, Yield 105 MPa
15200 psi
ASTM Data
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 42.3 µm/m-°C

@Temperature 20.0 °C
23.5 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 263 °C
505 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
Unannealed; ASTM Data
Vicat Softening Point 263 °C
505 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved