Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 131 µm/m-°C

@Temperature 20.0 °C
72.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
CTE, linear, Parallel to Flow 131 µm/m-°C

@Temperature 20.0 °C
72.8 µin/in-°F

@Temperature 68.0 °F
Covestro Texin® 4210 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w..