Polymer Property : CTE, linear, Parallel to Flow = 12.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES Elastoblend® PA6 GF25 IM L 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES Electrablend® PA12 CB
Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® ABS GF50 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® ABS GF60 BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 GF33 IM L UV 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier, Lubricant and UV StabilizerFeatures: Good UV Resistance, Impa..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 GF60 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill FR® PET GF15 IM FR X 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Impact Modifier and Mold ReleaseFeatures: Flame Retardant, Good Mold Release and Impact Modi..
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Techmer ES HiFill® ABS GF60 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc.