Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 20% Glass Reinforced
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Melting Point 254 °C
489 °F
Deflection Temperature at 0.46 MPa (66 psi) 243 °C
470 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
420 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149