Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 190 µm/m-°C @Temperature -30.0 - 120 °C |
106 µin/in-°F @Temperature -22.0 - 248 °F |
ISO 11359 |
Nyco NYLITE® Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur.. |
|||
CTE, linear, Parallel to Flow | 190 µm/m-°C @Temperature 20.0 °C |
106 µin/in-°F @Temperature 68.0 °F |
1 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
CTE, linear, Parallel to Flow | 190 µm/m-°C @Temperature 20.0 °C |
106 µin/in-°F @Temperature 68.0 °F |
1 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
CTE, linear, Parallel to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
CTE, linear, Parallel to Flow | 190 µm/m-°C @Temperature 23.0 - 250 °C |
106 µin/in-°F @Temperature 73.4 - 482 °F |
ASTM D696 |
Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled
(discontinued **) Data provided by the manufacturer.15 wt.% Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost n.. |