Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 0.700 µm/m-°C @Temperature 20.0 °C |
0.389 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® H950 Very high heat resistance,,Property data per ISO test methods. |
|||
CTE, linear, Parallel to Flow | 0.700 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.389 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |