Polymer Property : CTE, linear, Parallel to Flow = 0.389 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 0.700 µm/m-°C

@Temperature 20.0 °C
0.389 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H950
Very high heat resistance,,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.700 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.389 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR
LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive.