Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 136 J/g | 58.5 BTU/lb | |
Dow ISONATE™ 125M Pure MDI ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f.. |
|||
Heat of Fusion | 136 J/g | 58.5 BTU/lb | |
Dow ISONATE™ 125MDR Pure MDI ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers .. |