Polymer Property : Heat of Fusion = 136 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 136 J/g
58.5 BTU/lb
Dow ISONATE™ 125M Pure MDI
ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f..
Heat of Fusion 136 J/g
58.5 BTU/lb
Dow ISONATE™ 125MDR Pure MDI
ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers ..