Thermal Properties Metric English Comments
Heat of Fusion 60.0 J/g
25.8 BTU/lb
ASTM E793
Eastman CA12 PET  (discontinued **)
Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp..
Heat of Fusion 60.0 J/g
25.8 BTU/lb
ASTM E793
Eastman CB11E PET  (discontinued **)
VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet..