Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 52.0 J/g | 22.4 BTU/lb | Crystallinity; ExxonMobil Method |
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |