Material Notes:
Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:PP/TPO modification.EVA modification.Designed as a low density and high molecular weight polymer modifier to impart impact strength and toughness.Available as free flowing pellets.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAll physical properties were measured from specimens cut from compression molded plaques per ASTM D 4703, Procedure A, Type I and conditioned at 23°C for a minimum of 40 hours per ASTM D 618 prior to testing. All stress/strain tests used specimens cut with a Type IV (Die C) die and tested with a grip separation of 25 mm (1") and a crosshead speed of 20 in./min.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
ASTM D1505
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 68

@Time 15.0 sec
68

@Time 0.00417 hour
0.12 in; ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
ASTM D412 and ISO 37
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ASTM D412 and ISO 37
Elongation at Break 1500 %
1500 %
ASTM D412 and ISO 37
Flexural Modulus, 1% Secant 12.6 MPa
1830 psi
ASTM D790 and ISO 178
Thermal Properties Metric English Comments
Heat of Fusion 52.0 J/g
22.4 BTU/lb
Crystallinity; ExxonMobil Method
Melting Point 50.0 °C
122 °F
Peak; ExxonMobil Method
Crystallization Temperature 38.0 °C
100 °F
ExxonMobil Method
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525 and ISO 306/A
Glass Transition Temp, Tg -49.0 °C
-56.2 °F
ExxonMobil Method