Polymer Property : Heat of Fusion = 160 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 160 J/g
68.8 BTU/lb
DSC
Total 3802 YCF MDPE pipe grade
FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi..