Polymer Property : Heat of Fusion = 146 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 340 J/g
146 BTU/lb
AMT AM-Lite® Die Casting Magnesium Alloy
AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has..