Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 34.0 °C | 93.2 °F | |
3M 5425 UHMW Polyethylene Tape 3M™ UHMW Polyethylene Tape 5425 is a film coated with a special acrylic adhesive that is resistant to many solvents.Information provided by 3M |