3M 5425 UHMW Polyethylene Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5425 UHMW Polyethylene Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ UHMW Polyethylene Tape 5425 is a film coated with a special acrylic adhesive that is resistant to many solvents.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Backing; ASTM D3752
81.3 microns
3.20 mil
Liner; ASTM D3752
127 microns
5.00 mil
Total without liner; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.6 MPa
8790 psi
ASTM D3759
Elongation at Break 100 %
100 %
ASTM D3759
Peel Strength 0.3287 kN/m
1.875 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air 34.0 °C
93.2 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Translucent
Liner 55# densified kraft