Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 90.0 °C | 194 °F | |
3M Scotchcast™ 2104 Electrical Insulating Resin Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical.. |
|||
Minimum Service Temperature, Air | 90.0 °C | 194 °F | |
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin 3M Scotchcast Re-enterable Electrical Resin 2123 is a soft, two-part polybutadine resin encapsulant designed especially for re-enterable splice protection. It is formulated for virtually every elect.. |
|||
Minimum Service Temperature, Air | 90.0 °C | 194 °F | |
3M Scotchcast™ 2130 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it.. |