Polymer Property : Minimum Service Temperature, Air = 2.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Flat surfaces with and without rivets
3M Controltac™ 3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to surfaces with corrugations and rivets; Air release channels for fast, easy, bub..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Flat surfaces with and without rivets
3M Controltac™ 8652C Changeable Graphic Film with Comply™ Adhesive
Film 8652C is a 2-mil film with sideable, repositionable, pressure-activated adhesive. This short-term durable and removable film is an excellent choice for fleet graphics, including surfaces with c..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Flat surfaces with and without rivets
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Application
3M FP011902 Removable White Polypropylene Label Product
3M™ Removable White Polypropylene Label Product FP011902 is a glossy white opaque material that offers excellent durability and moisture resistance. This label product utilizes 3M™ Adhesive RMR10,..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Application
3M FV1172 Removable White Vinyl Label Products
3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive ..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Application
3M FV392 Removable White Vinyl Label Products
3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive ..
Minimum Service Temperature, Air 2.00 °C
35.6 °F
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer
This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering..