Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROLEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %
0.010 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 67.0 MPa
9720 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 30.0 MPa
4350 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
Melting Point 165 °C
329 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
130 °C
266 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75-2
Vicat Softening Point 90.0 °C
194 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air 2.00 °C
35.6 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A