Thermal Properties Metric English Comments
Minimum Service Temperature, Air 48.9 °C
120 °F
optimum use range
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally ..
Minimum Service Temperature, Air 48.9 °C
120 °F
Lower limit of working range
Heatbath/Park 400 Quench Oil
Similar to AAA but contains extra reservoir of accelerator additive for use in situations where excessive consumption occurs.Information provided by Heatbath Corporation - Park Metallurgical.