Polymer Property : Minimum Service Temperature, Air = -150 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -101 °C
-150 °F
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..