Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -101 °C | -150 °F | |
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |