Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 245 °C
473 °F
DSC on second heating cycle, Peak Melting Point; ASTM D3418
DAK Americas Laser+® MB912 PET
Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr..