Thermal Properties Metric English Comments
Crystallization Temperature 119 °C
246 °F
Petromont
Petromont 1100 High Density Polyethylene Resin
Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b..
Crystallization Temperature 119 °C
246 °F
Petromont
Petromont 2200 High Density Polyethylene Resin
Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr..
Crystallization Temperature 119 °C
246 °F
Dow Method (DSC)
Dow DMDA-8904 NT 7 High Density Polyethylene Resin
DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information..
Crystallization Temperature 119 °C
246 °F
Dow Method (DSC)
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..
Crystallization Temperature 119 °C
246 °F
Dow Method (DSC)
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous..
Crystallization Temperature 119 °C
246 °F
Dow Method (DSC)
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE)
Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme..