Polymer Property : Crystallization Temperature = 212 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 100 °C
212 °F
Dow Method (DSC)
Dow 620I Linear Low Density Polyethylene (LDPE)
For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Crystallization Temperature 100 °C
212 °F
Dow Method (DSC)
Dow 959S Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com..