Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 100 °C | 212 °F | Dow Method (DSC) |
Dow 620I Linear Low Density Polyethylene (LDPE) For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Crystallization Temperature | 100 °C | 212 °F | Dow Method (DSC) |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |