Thermal Properties Metric English Comments
Crystallization Temperature 48.0 - 52.0 °C
118 - 126 °F
Kazanorgsintez Oxanol CS-100
Production Method: Obtained by oxyethylation of primary alcohols of fractions C18-C20 obtained by alumoorganic synthesis. Application: Oxanol CS-100 is used for enzyme production in its pelletized f..
Crystallization Temperature >= 47.5 °C
>= 118 °F
A Grade
Shandong Dongyue Shenzhou New Material Co Perfluorooctanoic Acid (PFOA)
Conformable with: Q/DYS 006-2007PFOA is a strong organic acid, which has low surface tension and high surface activity, being used as surfactant, dispersant and additive. PFOA and its derivatives a..