Polymer Property : Vicat Softening Point = 97.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 - 97.0 °C
199 - 207 °F
ASTM D1525
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.