Polymer Property : Vicat Softening Point = 94.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 94.4 °C
202 °F
annealed; ASTM D-1525A
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..
Vicat Softening Point 94.4 °C
202 °F
ASTM D1525
American Polymers API 425 Polystyrene
API 425 is a medium impact grade of polystyrene for injection molding. API 425 has good gloss, easy flow and fast cycling properties.Applications: API 425 is widely used in cosmetic packaging, food..