Polymer Property : Vicat Softening Point = 84.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 241 Rigid PVC, Extrusion
Various profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 324 Rigid PVC, Extrusion
Furniture profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 330 Rigid PVC, Extrusion
Various profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 425 Rigid PVC, Extrusion
Electric channels
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 425/R Rigid PVC, Extrusion
Shiny electric channels
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion
Antishock pipes and profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 4410 Rigid PVC, Antishock Extrusion
Antishock spiral pipes
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free
Rolling shutters
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 325 Rigid PVC, Extrusion Lead Free
Verticle curtains
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free
Profiles anti mould
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free
Profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 435 Rigid PVC, Extrusion Lead Free
Electrical channels
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds R 211 Rigid PVC, Extrusion
Shutters and shiny profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds R 218 Rigid PVC, Extrusion
Shutters and shiny profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds R 316 Rigid PVC, Extrusion
Rolling shutters
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds R 316/AS Rigid PVC, Extrusion
Antistatic profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 121 Rigid PVC, Extrusion
Electric pipes
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds R 212/C Rigid PVC, Extrusion
Shutters and shiny profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 140/1 Rigid PVC, Extrusion
Drain-pipes
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 224 Rigid PVC, Extrusion
Various profiles
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 430 Rigid PVC, Extrusion
Electric channels
Vicat Softening Point 82.0 - 84.0 °C

@Load 5.00 kg
180 - 183 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 230/D Rigid PVC, Extrusion
Electric channels