Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 40.0 - 74.0 °C | 104 - 165 °F | Average value: 60.4 °C Grade Count:39 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Vicat Softening Point | 72.0 - 74.0 °C @Load 5.00 kg |
162 - 165 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 52/C Rigid PVC, Injection Molding Electric fittings |