Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 71.1 °C | 160 °F | ASTM D1525 |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |
|||
Vicat Softening Point | 71.1 °C | 160 °F | ASTM D1525 |
ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide .. |