Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 69.0 - 71.0 °C @Load 5.00 kg |
156 - 160 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 50 Rigid PVC, Injection Molding Technical items |
|||
Vicat Softening Point | 39.0 - 71.0 °C | 102 - 160 °F | Average value: 52.1 °C Grade Count:7 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |