Polymer Property : Vicat Softening Point = 160 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 69.0 - 71.0 °C

@Load 5.00 kg
156 - 160 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RI 50 Rigid PVC, Injection Molding
Technical items
Vicat Softening Point 39.0 - 71.0 °C
102 - 160 °F
Average value: 52.1 °C Grade Count:7
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..