Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 335 °C @Load 1.02 kg |
635 °F @Load 2.25 lb |
Method A; ISO 306 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Vicat Softening Point | 335 °C @Load 1.02 kg |
635 °F @Load 2.25 lb |
Method A; ISO 306 |
Westlake Plastics MediPEEK T Polyetheretherketone for Medical Applications MediPEEK-T is a high performance semi-crystalline thermoplastic designed for short term body contact as an implantable material. It is USP Class VI and ASTM F2026 compliant. It has excellent steri.. |