Polymer Property : Vicat Softening Point = 335 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 335 °C

@Load 1.02 kg
635 °F

@Load 2.25 lb
Method A; ISO 306
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications
MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st..
Vicat Softening Point 335 °C

@Load 1.02 kg
635 °F

@Load 2.25 lb
Method A; ISO 306
Westlake Plastics MediPEEK T Polyetheretherketone for Medical Applications
MediPEEK-T is a high performance semi-crystalline thermoplastic designed for short term body contact as an implantable material. It is USP Class VI and ASTM F2026 compliant. It has excellent steri..