Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 270 - 290 °C | 518 - 554 °F | Average value: 280 °C Grade Count:9 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Vicat Softening Point | 270 °C | 518 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Vicat Softening Point | 270 °C @Load 5.00 kg |
518 °F @Load 11.0 lb |
|
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Vicat Softening Point | 270 °C @Load 5.00 kg |
518 °F @Load 11.0 lb |
|
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C | 518 °F | ASTM D1525 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Vicat Softening Point | 270 °C @Load 5.00 kg |
518 °F @Load 11.0 lb |
|
LATI Latilub 88/50-20T PEEK, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Vicat Softening Point | 270 - 295 °C | 518 - 563 °F | Average value: 287 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |