Polymer Property : Vicat Softening Point = 480 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 249 °C
480 °F
ASTM D1525
PlastxWorld Veroplas PB3301F Nylon 66
flame retarded (UL94 V0), 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 249 °C
480 °F
ASTM D1525
PlastxWorld Veroplas PB3400 Nylon 66
general purpose, 40% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 249 °C
480 °F
ASTM D1525
PlastxWorld Veroplas PB3500 Nylon 66
general purpose, 50% glass filled injection molding gradeInformation provided by PlastxWorld Inc.