PlastxWorld Veroplas PB3500 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PB3500 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
general purpose, 50% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 220 MPa
31900 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 265 MPa
38400 psi
ASTM D790
Flexural Modulus 9.501 GPa
1378 ksi
ASTM D790
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Vicat Softening Point 249 °C
480 °F
ASTM D1525
Glow Wire Test 649 °C
1200 °F
UNE 20-672-83