Thermal Properties Metric English Comments
Vicat Softening Point 48.3 °C
119 °F
ASTM D1525
ExxonMobil Escorene™ FL 02020 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 02020 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 02020 is an excellent sealing materi..
Vicat Softening Point 48.3 °C
119 °F
ASTM D1525
ExxonMobil Escorene™ UL 02020 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 02020 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation.Availability: Africa & Mid..