Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 02020 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 02020 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 02020 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Adhesives and SealantsInjection Molding Wire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 20 %
20 %
ExxonMobil method
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0262 GPa
3.80 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 174 °C
<= 345 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 48.3 °C
119 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 240